• T-PUT Welding Rod Thermanit P 23
Thermanit P 23 description: Basic covered medium alloyed electrode for the welding of similar creep resistant materials. Good welding characteristics even in out-of-postion welding. Redry for 2h at 300 - 350 °C ( 572 - 662 °F).