Thermanit JE-308L description: Stainless; resistant to intercrystalline corrosion and wet corrosion up to 350 °C (662 °F). Corrosion-resistant similar to matching low-carbon and stabilized austenitic 18/8 CrNi(N) steels/cast steel grades. High toughness at subzero temperatures as low as –196 °C (–321 °F). For joning and surfacing applications with matching and similar-stabilized and non-stabilized – austenitic CrNi(N) and CrNiMo(N) steels/cast steel grades. For joining and surfacing work on cryogenic matching/similar austenitic CrNi(N) steels/cast steel grades.